Google+ post by Aria C Bramanta on 2016-05-10 18:13:45 UTC

Nylon prints

It warped, I had to replace my aluminum bed with canvas(untreated) embedded with two part epoxy with onyx powder filling for a good mechanical and chemical adhesion

What sort of nylon are you printing? I print Taulman Bridge on heated glass (50C) covered with UHU stic. No issues at all with adhesion.

I use Taulman 618, and canvas embedded two part epoxy bed, heats it up to 60-70°c, uhu doesn’t work for me (on glass or aluminum)

Interesting. I had a large box of sticks, and am down to 2. I have ordered another box and will be interested if it works just as well, and will report somewhere here is anyone is interested.

Maybe it comes with different chemical compound here, I don’t know…but I do know oem printers comes with phenolic canvas, or garolite bed (such as the mark one)